The Lead-Tin vacuum distillation unit (Pb Sn Sb VDF) separates Tin from lead alloy, a byproduct of lead smelting. It uses varying boiling points of Tin, Antimony, and Lead under vacuum to remove impurities.
Operating under the vacuum, the Sn VDF creates distinct boiling points for different metals. The vapors of lead and tin condense at different locations, forming liquid lead and tin.
The VDF relies on electricity for heat and operates without emitting gases, making it environmentally preferable. It includes a method for collecting arsenic at low concentrations (As≤1%). If arsenic content exceeds a certain threshold (As≥2%), it must be removed before furnace use.
When it's under vacuum, the Pb-Sn-Sb VDF makes different metals boil at different points. Inside the Pb-Sn-Sb VDF's graphite tray, the vapors of lead and tin move to different spots, and turn into liquid lead and tin.
The Pb-Sn-Sb VDF uses electricity for heat, and it doesn't let out any gases while working, which makes it better for the environment. It also has a way to collect arsenic when there's not too much of it(As≤1%). If there's too much arsenic(As≥2%), it needs to be removed before using the furnace.
1) Furnace body
2) Constant feeder
3) Melting furnace
4) Operating platform
5) Electric control cabinet
6) Gas circuit system
7) Water circuit system
8) Vacuum casting chamber
9) Pb holding furnace
10) Power source
Raw material:
S/N | Material | Remark |
1. | Lead-Tin alloy |
|
2. | Soldering Tin |
|
3. | Lead-Tin-Antimony alloy |
|
4. | Lead-Tin-Antimony-Arsenic alloy | As≤0.4 |
5. | Crude Tin |
|
Main parameters:
NO. | Item | Index |
1 | Treating capacity (raw material) | 15~10t/d |
2 | Vacuum degree | 10-30 Pa |
3 | Recovery rate of Tin | 99% |
4 | Recovery rate of Lead | 99% |
5 | Power | 100 kW |
6 | Energy consumption | ≤950 kWh/t |
FAQ:
Q1: What's payment terms are acceptable?
A: LC, TT and cash.
Q2: Can you provide installation service?
A: Yes, we provide the clients with installation service or installation instruction through online or other methods as per their needs.
Q3: Can you provide design service to client?
A: Yes, we can provide customized design services and Pb-Sn-Sb VDF as per clients' needs.
Q4: What are the raw materials and final product of the Pb-Sn-Sb VDF?
A: The raw materials are the lead-tin alloy, The final product is crude tin (≥985.% Sn). This crude tin can easily be refined using crystallizer and/or impurity-removing pot.
Q5: Does the Pb-Sn-Sb VDF can work alone?
A: Yes. The output product, crude tin, can be sold as merchandise.
Relevant processes: lead-tin separation, tin extraction, lead-tin-antimony vacuum distillation furnace, lead-tin alloy treatment, lead-acid battery recovery slag treatment, crude lead refining, Pb-Sn VDF, vacuum distillation, tin refining,Pb-Sn-Sb VDF.